Chinese JoineryChinese Joinery
Wood

White oak wood

White oak is a medium-hard hardwood2: 1,360 lbf1 on the Janka side-hardness test at 12% moisture, above northern red oak (1,290 lbf3) and below sugar maple (1,450 lbf3).

It is moderately stiff4, and it moves about 0.38%5 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyWhite oak
Janka hardness, 12% MC1,360 lbf1; 6,000 N6
Janka hardness, green1,060 lbf1
Specific gravity, 12% MC volume basis0.681
Bending strength (MOR), 12% MC15,200 psi1; 105,000 kPa6
Stiffness (MOE), 12% MC1.78 × 106 psi1; 12,300 MPa6
Shrinkage, green to oven-dryradial 5.6%, tangential 10.5%, volumetric 16.3%7
T/R ratio (tangential ÷ radial)1.88, calculated8
Movement coefficientsCR 0.00194; CT 0.003765

How hard is white oak?

01,0002,0003,0004,000white oak 1,360 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See white oak on the Janka chart.

How much does it move?

A 10-inch flat-sawn white oak board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States10, widens by 0.150 in9. A quartersawn board widens by 0.078 in9.

The coefficients apply from 6% to 14% moisture content11.

Try your own board in the wood movement calculator.

What it's used for

White oak is a principal species of the white oak group. The sapwood is nearly white and the heartwood is generally grayish brown; the pores are usually plugged, so most white oaks suit tight cooperage, and the heartwood resists decay. It is used for lumber, ties, cooperage, furniture, flooring, doors, millwork, and planking and bent parts of ships and boats.12

Compare with

Questions

Is white oak a hardwood?
Yes. White oak is a hardwood13. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a 12% MC volume basis is 0.681.
Is white oak harder than northern red oak?
White oak is harder than northern red oak: 1,360 lbf1 versus 1,290 lbf3, both at 12% moisture.
How much does white oak shrink?
From green to oven-dry, tangential shrinkage is 10.5% and radial shrinkage is 5.6%7. The T/R ratio is 1.88, calculated8.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-10
  • 4. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 5. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
  • 6. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-6
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
  • 8. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
  • 9. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00376; radial coefficient 0.00194.
  • 10. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 11. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-9
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2