Chinese JoineryChinese Joinery
Wood

Teak wood

Teak is a medium-hard hardwood2: 1,000 lbf1 on the Janka side-hardness test at 12% moisture, almost the same as black walnut (1,010 lbf4) and almost the same as black cherry (950 lbf3).

It is flexible5, and it moves about 0.20%6 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyTeak
Janka hardness, 12% MC1,000 lbf1; 4,400 N7
Janka hardness, green930 lbf1
Specific gravity, green volume basis0.551
Bending strength (MOR), 12% MC14,600 psi1; 100,700 kPa7
Stiffness (MOE), 12% MC1.55 × 106 psi1; 10,700 MPa7
Shrinkage, green to oven-dryradial 2.5%, tangential 5.8%, volumetric 7%8
T/R ratio (tangential ÷ radial)2.32, calculated9
Movement coefficientsCR 0.00085, calculated; CT 0.00201, calculated6

How hard is teak?

01,0002,0003,0004,000teak 1,000 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See teak on the Janka chart.

How much does it move?

A 10-inch flat-sawn teak board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States11, widens by 0.080 in10. A quartersawn board widens by 0.034 in10.

The coefficients apply from 6% to 14% moisture content12.

Try your own board in the wood movement calculator.

What it's used for

The heartwood varies from yellow-brown to dark golden brown and eventually turns a rich brown on exposure. The texture is coarse and uneven, the grain is usually straight, and the wood has an oily feel; it is generally worked with moderate ease, though silica often dulls tools. It is used for boats, furniture, flooring, decorative objects, and decorative veneer, and in shipbuilding where it meets metal.13

Compare with

Questions

Is teak a hardwood?
Yes. Teak is a hardwood14. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a green volume basis is 0.551.
Is teak harder than black walnut?
Teak is softer than black walnut: 1,000 lbf1 versus 1,010 lbf4, both at 12% moisture.
How much does teak shrink?
From green to oven-dry, tangential shrinkage is 5.8% and radial shrinkage is 2.5%8. The T/R ratio is 2.32, calculated9.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-25
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
  • 4. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
  • 5. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 6. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-21
  • 8. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
  • 9. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).
  • 10. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00201; radial coefficient 0.00085.
  • 11. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-38
  • 14. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2