Oak vs Teak wood
Northern red oak (red oak group) is harder and stiffer than teak but weaker in bending: 1,2901 vs 1,0002 lbf, 29% harder3. White oak (white oak group) is harder, stronger in bending and stiffer than teak: 1,3604 vs 1,0002 lbf, 36% harder3. Teak moves less across a flat-sawn board (CT 0.002015 vs 0.003046 and 0.003766). Northern red oak and white oak are denser (specific gravity 0.561 and 0.64 vs 0.552, green volume basis).
Side by side
| Property | Northern red oak (red oak group) | White oak (white oak group) | Teak |
|---|---|---|---|
| Janka hardness, 12% MC | 1,290 lbf1; 5,700 N7 | 1,360 lbf4; 6,000 N8 | 1,000 lbf2; 4,400 N9 |
| Janka hardness, green | 1,000 lbf1 | 1,060 lbf4 | 930 lbf2 |
| Specific gravity, green volume basis | 0.561 | 0.64 | 0.552 |
| Bending strength (MOR), 12% MC | 14,300 psi1; 99,000 kPa7 | 15,200 psi4; 105,000 kPa8 | 14,600 psi2; 100,700 kPa9 |
| Stiffness (MOE), 12% MC | 1.82 × 106 psi1; 12,500 MPa7 | 1.78 × 106 psi4; 12,300 MPa8 | 1.55 × 106 psi2; 10,700 MPa9 |
| Shrinkage, green to oven-dry | radial 4%, tangential 8.6%, volumetric 13.7%10 | radial 5.6%, tangential 10.5%, volumetric 16.3%10 | radial 2.5%, tangential 5.8%, volumetric 7%11 |
| T/R ratio (tangential ÷ radial) | 2.15, calculated12 | 1.88, calculated12 | 2.32, calculated13 |
| Movement coefficients | CR 0.00137; CT 0.003046 | CR 0.00194; CT 0.003766 | CR 0.00085, calculated; CT 0.00201, calculated5 |
Which to use
For a tabletop that must resist dents, white oak (white oak group) is the harder wood at 1,360 lbf4, against teak at 1,000 lbf2.
For a wide flat-sawn panel, teak moves less (CT 0.002015, against white oak at 0.003766).
Related
Questions
- Is oak harder than teak?
- Yes. Northern red oak (red oak group) at 1,290 lbf1 and white oak (white oak group) at 1,360 lbf4 are harder than teak at 1,000 lbf2.
- Which moves more, oak or teak?
- Northern red oak (red oak group) and white oak (white oak group) move more than teak across a flat-sawn board (CT 0.003046 and CT 0.003766 vs CT 0.002015).
References
- 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-10
- 2. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-25
- 3. Calculated from the two 12% Janka values: the difference divided by the lower value.
- 4. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
- 5. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
- 6. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
- 7. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-5
- 8. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-6
- 9. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-21
- 10. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
- 11. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
- 12. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
- 13. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).