Spanish cedar wood
Spanish cedar (Spanish-cedar, Cedrela spp.) is a medium-soft hardwood2: 600 lbf1 on the Janka side-hardness test at 12% moisture, above yellow-poplar (540 lbf3) and well below black cherry (950 lbf4).
It is flexible5, and it moves about 0.22%6 across the width of a flat-sawn board for each 1% change in moisture content.
Key numbers
| Property | Spanish-cedar |
|---|---|
| Janka hardness, 12% MC | 600 lbf1; 2,700 N7 |
| Janka hardness, green | 550 lbf1 |
| Specific gravity, green volume basis | 0.411 |
| Bending strength (MOR), 12% MC | 11,500 psi1; 79,300 kPa7 |
| Stiffness (MOE), 12% MC | 1.44 × 106 psi1; 9,900 MPa7 |
| Shrinkage, green to oven-dry | radial 4.2%, tangential 6.3%, volumetric 10.3%8 |
| T/R ratio (tangential ÷ radial) | 1.50, calculated9 |
| Movement coefficients | CR 0.00144, calculated; CT 0.00219, calculated6 |
How hard is Spanish cedar?
Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See Spanish-cedar on the Janka chart.
How much does it move?
A 10-inch flat-sawn Spanish-cedar board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States11, widens by 0.088 in10. A quartersawn board widens by 0.058 in10.
The coefficients apply from 6% to 14% moisture content12.
Try your own board in the wood movement calculator.
What it's used for
The heartwood varies from light to dark reddish brown and the sapwood is pinkish to white. The texture runs from rather fine and uniform to coarse and uneven, the grain is not interlocked, and the heartwood has a distinctive odor; the wood dries easily and works and glues well. It is favored for millwork, cabinets, fine furniture, boat building, cigar boxes, humidors, and plywood.13
Compare with
Questions
- Is Spanish cedar a hardwood?
- Yes. Spanish cedar is a hardwood14. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a green volume basis is 0.411.
- Is Spanish cedar harder than yellow-poplar?
- Spanish cedar is harder than yellow-poplar: 600 lbf1 versus 540 lbf3, both at 12% moisture.
- How much does Spanish cedar shrink?
- From green to oven-dry, tangential shrinkage is 6.3% and radial shrinkage is 4.2%8. The T/R ratio is 1.50, calculated9.
References
- 1. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-25
- 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
- 4. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
- 5. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 6. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
- 7. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-21
- 8. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
- 9. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).
- 10. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00219; radial coefficient 0.00144.
- 11. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
- 12. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
- 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-37
- 14. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2