Chinese JoineryChinese Joinery
Wood

Loblolly pine wood

Loblolly pine is a medium-soft softwood2: 690 lbf1 on the Janka side-hardness test at 12% moisture, above yellow-poplar (540 lbf3) and below black cherry (950 lbf4).

It is moderately stiff5, and it moves about 0.26%6 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyLoblolly pine
Janka hardness, 12% MC690 lbf1; 3,100 N7
Janka hardness, green450 lbf1
Specific gravity, 12% MC volume basis0.511
Bending strength (MOR), 12% MC12,800 psi1; 88,000 kPa7
Stiffness (MOE), 12% MC1.79 × 106 psi1; 12,300 MPa7
Shrinkage, green to oven-dryradial 4.8%, tangential 7.4%, volumetric 12.3%8
T/R ratio (tangential ÷ radial)1.54, calculated9
Movement coefficientsCR 0.00165; CT 0.002596

How hard is loblolly pine?

01,0002,0003,0004,000loblolly pine 690 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See loblolly pine on the Janka chart.

How much does it move?

A 10-inch flat-sawn loblolly pine board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States11, widens by 0.104 in10. A quartersawn board widens by 0.066 in10.

The coefficients apply from 6% to 14% moisture content12.

Try your own board in the wood movement calculator.

What it's used for

Southern pine sapwood is yellowish white and the heartwood is reddish brown. The lumber is used for building material, boxes, pallets, crates, and cooperage, and denser stock is used for heavy construction.13

Compare with

Questions

Is loblolly pine a hardwood?
No. Loblolly pine is a softwood14. Softwoods are conifers. The name is botanical, not a hardness ranking. Specific gravity on a 12% MC volume basis is 0.511.
Is loblolly pine harder than yellow-poplar?
Loblolly pine is harder than yellow-poplar: 690 lbf1 versus 540 lbf3, both at 12% moisture.
How much does loblolly pine shrink?
From green to oven-dry, tangential shrinkage is 7.4% and radial shrinkage is 4.8%8. The T/R ratio is 1.54, calculated9.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-12
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
  • 4. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
  • 5. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 6. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-7
  • 8. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
  • 9. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
  • 10. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00259; radial coefficient 0.00165.
  • 11. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-15
  • 14. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2