Eastern red cedar wood
Eastern red cedar (eastern redcedar, Juniperus virginiana) is a softwood. The Handbook prints side hardness at 12% moisture as 4,000 N1 and prints no pound-force figure. That is ≈ 900 lbf, calculated2, and it is not placed on the 12% pound-force ranking.
It is flexible3, and it moves about 0.16%4 across the width of a flat-sawn board for each 1% change in moisture content.
Key numbers
| Property | Eastern redcedar |
|---|---|
| Janka hardness, 12% MC | 4,000 N1; ≈ 900 lbf, calculated2 |
| Janka hardness, green | 650 lbf5 |
| Specific gravity, 12% MC volume basis | 0.475 |
| Bending strength (MOR), 12% MC | 8,800 psi5; 61,000 kPa1 |
| Stiffness (MOE), 12% MC | 0.88 × 106 psi5; 6,100 MPa1 |
| Shrinkage, green to oven-dry | radial 3.1%, tangential 4.7%, volumetric 7.8%6 |
| T/R ratio (tangential ÷ radial) | 1.52, calculated7 |
| Movement coefficients | CR 0.00106; CT 0.001624 |
How much does it move?
A 10-inch flat-sawn eastern redcedar board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States9, widens by 0.065 in8. A quartersawn board widens by 0.042 in8.
The coefficients apply from 6% to 14% moisture content10.
Try your own board in the wood movement calculator.
What it's used for
The heartwood is bright or dull red, the narrow sapwood is nearly white, and the texture is fine and uniform. Shrinkage is very low and the heartwood resists decay. The greatest use is fence posts; lumber is made into chests, wardrobes, and closet lining, and other uses include flooring, novelties, pencils, and small boats.11
Compare with
Questions
- Is eastern red cedar a hardwood?
- No. Eastern red cedar is a softwood12. Softwoods are conifers. The name is botanical, not a hardness ranking. Specific gravity on a 12% MC volume basis is 0.475.
- What is the Janka hardness of eastern red cedar?
- At 12% moisture the Handbook prints 4,000 N1 and no pound-force value. That is ≈ 900 lbf, calculated2.
- How much does eastern red cedar shrink?
- From green to oven-dry, tangential shrinkage is 4.7% and radial shrinkage is 3.1%6. The T/R ratio is 1.52, calculated7.
References
- 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-6
- 2. Calculated from 4,000 N in USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-6, using 1 lbf = 4.448 N (≈ 900 lbf). Not used in the 12% ranking.
- 3. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 4. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
- 5. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
- 6. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
- 7. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
- 8. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00162; radial coefficient 0.00106.
- 9. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
- 10. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
- 11. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-17
- 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2