Chinese JoineryChinese Joinery
Wood

Sycamore (American sycamore) wood

Sycamore (American sycamore, Platanus occidentalis) is a medium-soft hardwood2: 770 lbf1 on the Janka side-hardness test at 12% moisture, below black cherry (950 lbf3) and above yellow-poplar (540 lbf1).

It is flexible4, and it moves about 0.30%5 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyAmerican sycamore
Janka hardness, 12% MC770 lbf1; 3,400 N6
Janka hardness, green610 lbf1
Specific gravity, 12% MC volume basis0.491
Bending strength (MOR), 12% MC10,000 psi1; 69,000 kPa6
Stiffness (MOE), 12% MC1.42 × 106 psi1; 9,800 MPa6
Shrinkage, green to oven-dryradial 5%, tangential 8.4%, volumetric 14.1%7
T/R ratio (tangential ÷ radial)1.68, calculated8
Movement coefficientsCR 0.00172; CT 0.002975

How hard is sycamore (American sycamore)?

01,0002,0003,0004,000American sycamore 770 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See American sycamore on the Janka chart.

How much does it move?

A 10-inch flat-sawn American sycamore board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States10, widens by 0.119 in9. A quartersawn board widens by 0.069 in9.

The coefficients apply from 6% to 14% moisture content11.

Try your own board in the wood movement calculator.

What it's used for

The heartwood is reddish brown and the sapwood is light in color. The wood has a fine texture and interlocked grain. It is used for lumber, veneer, ties, and slack cooperage; the lumber goes into furniture, boxes, pallets, flooring, handles, and butcher blocks.12

Compare with

Questions

Is sycamore a hardwood?
Yes. Sycamore is a hardwood13. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a 12% MC volume basis is 0.491.
Is sycamore harder than black cherry?
Sycamore is softer than black cherry: 770 lbf1 versus 950 lbf3, both at 12% moisture.
How much does sycamore shrink?
From green to oven-dry, tangential shrinkage is 8.4% and radial shrinkage is 5%7. The T/R ratio is 1.68, calculated8.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
  • 4. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 5. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
  • 6. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-6
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
  • 8. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
  • 9. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00297; radial coefficient 0.00172.
  • 10. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 11. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-10
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2