Chinese JoineryChinese Joinery
Wood

Purpleheart wood

Purpleheart is a hardwood, hard on the Janka scale2: 1,860 lbf1 on the Janka side-hardness test at 12% moisture, almost the same as shagbark hickory (1,880 lbf3) and above sugar maple (1,450 lbf3).

It is stiff4, and it moves about 0.21%5 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyPurpleheart
Janka hardness, 12% MC1,860 lbf1; 8,300 N6
Janka hardness, green1,810 lbf1
Specific gravity, green volume basis0.671
Bending strength (MOR), 12% MC19,200 psi1; 132,400 kPa6
Stiffness (MOE), 12% MC2.27 × 106 psi1; 15,700 MPa6
Shrinkage, green to oven-dryradial 3.2%, tangential 6.1%, volumetric 9.9%7
T/R ratio (tangential ÷ radial)1.91, calculated8
Movement coefficientsCR 0.00109, calculated; CT 0.00212, calculated5

How hard is purpleheart?

01,0002,0003,0004,000purpleheart 1,860 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See purpleheart on the Janka chart.

How much does it move?

A 10-inch flat-sawn purpleheart board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States10, widens by 0.085 in9. A quartersawn board widens by 0.044 in9.

The coefficients apply from 6% to 14% moisture content11.

Try your own board in the wood movement calculator.

What it's used for

Freshly cut heartwood is brown, turns a deep purple on exposure to air, and eventually turns dark brown in the light. The texture is medium to fine and the grain is usually straight; the wood is moderately difficult to work and dulls cutters, but it turns easily and takes finishes well. The color makes it desirable for turnery, marquetry, cabinets, fine furniture, and parquet flooring.12

Compare with

Questions

Is purpleheart a hardwood?
Yes. Purpleheart is a hardwood13. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a green volume basis is 0.671.
Is purpleheart harder than shagbark hickory?
Purpleheart is softer than shagbark hickory: 1,860 lbf1 versus 1,880 lbf3, both at 12% moisture.
How much does purpleheart shrink?
From green to oven-dry, tangential shrinkage is 6.1% and radial shrinkage is 3.2%7. The T/R ratio is 1.91, calculated8.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-24
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-10
  • 4. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 5. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
  • 6. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-20
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
  • 8. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).
  • 9. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00212; radial coefficient 0.00109.
  • 10. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 11. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-34
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2