Okoume wood
Okoume is a soft hardwood2: 380 lbf1 on the Janka side-hardness test at 12% moisture, below yellow-poplar (540 lbf3).
It is flexible4, and it moves about 0.21%5 across the width of a flat-sawn board for each 1% change in moisture content.
Key numbers
| Property | Okoume |
|---|---|
| Janka hardness, 12% MC | 380 lbf1; 1,700 N6 |
| Specific gravity, green volume basis | 0.331 |
| Bending strength (MOR), 12% MC | 7,400 psi1; 51,000 kPa6 |
| Stiffness (MOE), 12% MC | 1.14 × 106 psi1; 7,900 MPa6 |
| Shrinkage, green to oven-dry | radial 4.1%, tangential 6.1%, volumetric 11.3%7 |
| T/R ratio (tangential ÷ radial) | 1.49, calculated8 |
| Movement coefficients | CR 0.00141, calculated; CT 0.00212, calculated5 |
How hard is okoume?
Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See okoume on the Janka chart.
How much does it move?
A 10-inch flat-sawn okoume board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States10, widens by 0.085 in9. A quartersawn board widens by 0.056 in9.
The coefficients apply from 6% to 14% moisture content11.
Try your own board in the wood movement calculator.
What it's used for
The heartwood is salmon-pink, the narrow sapwood is whitish or pale gray, and the wood has a high luster and a uniform texture slightly coarser than birch. Sawn lumber is somewhat difficult to machine because of silica, but the wood glues and peels into veneer easily. In the United States it is used for decorative plywood paneling, utility plywood, doors, furniture components, and joinery.12
Compare with
Questions
- Is okoume a hardwood?
- Yes. Okoume is a hardwood13. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a green volume basis is 0.331.
- Is okoume harder than eastern white pine?
- Okoume is the same hardness as eastern white pine: 380 lbf1 versus 380 lbf14, both at 12% moisture.
- How much does okoume shrink?
- From green to oven-dry, tangential shrinkage is 6.1% and radial shrinkage is 4.1%7. The T/R ratio is 1.49, calculated8.
References
- 1. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-24
- 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
- 4. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 5. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
- 6. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-20
- 7. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
- 8. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).
- 9. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00212; radial coefficient 0.00141.
- 10. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
- 11. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
- 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-32
- 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2
- 14. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-12