Chinese JoineryChinese Joinery
Wood

Butternut wood

Butternut is a soft hardwood2: 490 lbf1 on the Janka side-hardness test at 12% moisture, almost the same as yellow-poplar (540 lbf4) and above eastern white pine (380 lbf3).

It is flexible5, and it moves about 0.22%6 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyButternut
Janka hardness, 12% MC490 lbf1; 2,200 N7
Janka hardness, green390 lbf1
Specific gravity, 12% MC volume basis0.381
Bending strength (MOR), 12% MC8,100 psi1; 56,000 kPa7
Stiffness (MOE), 12% MC1.18 × 106 psi1; 8,100 MPa7
Shrinkage, green to oven-dryradial 3.4%, tangential 6.4%, volumetric 10.6%8
T/R ratio (tangential ÷ radial)1.88, calculated9
Movement coefficientsCR 0.00116; CT 0.002236

How hard is butternut?

01,0002,0003,0004,000butternut 490 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See butternut on the Janka chart.

How much does it move?

A 10-inch flat-sawn butternut board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States11, widens by 0.089 in10. A quartersawn board widens by 0.046 in10.

The coefficients apply from 6% to 14% moisture content12.

Try your own board in the wood movement calculator.

What it's used for

The narrow sapwood is nearly white and the heartwood is light brown, often with pinkish tones or darker brown streaks. The texture is rather coarse; the wood machines easily, finishes well, and can resemble black walnut especially when stained. Lumber and veneer are made into furniture, cabinets, paneling, and interior woodwork.13

Compare with

Questions

Is butternut a hardwood?
Yes. Butternut is a hardwood14. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a 12% MC volume basis is 0.381.
Is butternut harder than yellow-poplar?
Butternut is softer than yellow-poplar: 490 lbf1 versus 540 lbf4, both at 12% moisture.
How much does butternut shrink?
From green to oven-dry, tangential shrinkage is 6.4% and radial shrinkage is 3.4%8. The T/R ratio is 1.88, calculated9.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-12
  • 4. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-11
  • 5. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 6. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-4
  • 8. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
  • 9. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
  • 10. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00223; radial coefficient 0.00116.
  • 11. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-5
  • 14. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2