Chinese JoineryChinese Joinery
Wood

Bubinga wood

Bubinga is a very hard hardwood2: 2,690 lbf1 on the Janka side-hardness test at 12% moisture, above shagbark hickory (1,880 lbf3) and below ipe (3,680 lbf4).

It is stiff5, and it moves about 0.30%6 across the width of a flat-sawn board for each 1% change in moisture content.

Key numbers

PropertyBubinga
Janka hardness, 12% MC2,690 lbf1; 12,000 N7
Specific gravity, green volume basis0.711
Bending strength (MOR), 12% MC22,600 psi1; 155,800 kPa7
Stiffness (MOE), 12% MC2.48 × 106 psi1; 17,100 MPa7
Shrinkage, green to oven-dryradial 5.8%, tangential 8.4%, volumetric 14.2%8
T/R ratio (tangential ÷ radial)1.45, calculated9
Movement coefficientsCR 0.00201, calculated; CT 0.00297, calculated6

How hard is bubinga?

01,0002,0003,0004,000bubinga 2,690 lbf

Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See bubinga on the Janka chart.

How much does it move?

A 10-inch flat-sawn bubinga board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States11, widens by 0.119 in10. A quartersawn board widens by 0.080 in10.

The coefficients apply from 6% to 14% moisture content12.

Try your own board in the wood movement calculator.

What it's used for

Bubinga heartwood is pink, vivid red, or red-brown with purple streaks, and on exposure it becomes yellow or medium brown with a reddish tint. The texture is fine to moderately fine. It can be worked well with hand and machine tools, and it is used for turnery, flooring, furniture components, cabinetwork, and decorative veneers.13

Compare with

Questions

Is bubinga a hardwood?
Yes. Bubinga is a hardwood14. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a green volume basis is 0.711.
Is bubinga harder than shagbark hickory?
Bubinga is harder than shagbark hickory: 2,690 lbf1 versus 1,880 lbf3, both at 12% moisture.
How much does bubinga shrink?
From green to oven-dry, tangential shrinkage is 8.4% and radial shrinkage is 5.8%8. The T/R ratio is 1.45, calculated9.

References

  • 1. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-22
  • 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-10
  • 4. USDA Wood Handbook (FPL-GTR-282), Table 5-5b, p. 5-23
  • 5. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
  • 6. Calculated with Wood Handbook Eq. 13-2 (p. 13-16) from Table 4-4 (p. 4-9)
  • 7. USDA Wood Handbook (FPL-GTR-282), Table 5-5a, p. 5-18
  • 8. USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9
  • 9. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-4, p. 4-9).
  • 10. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00297; radial coefficient 0.00201.
  • 11. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
  • 12. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
  • 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-22
  • 14. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2