Aspen (quaking aspen) wood
Aspen (quaking aspen, Populus tremuloides) is a soft hardwood2: 350 lbf1 on the Janka side-hardness test at 12% moisture, almost the same as eastern white pine (380 lbf3).
It is flexible4, and it moves about 0.23%5 across the width of a flat-sawn board for each 1% change in moisture content.
Key numbers
| Property | Quaking aspen |
|---|---|
| Janka hardness, 12% MC | 350 lbf1; 1,600 N6 |
| Janka hardness, green | 300 lbf1 |
| Specific gravity, 12% MC volume basis | 0.381 |
| Bending strength (MOR), 12% MC | 8,400 psi1; 58,000 kPa6 |
| Stiffness (MOE), 12% MC | 1.18 × 106 psi1; 8,100 MPa6 |
| Shrinkage, green to oven-dry | radial 3.5%, tangential 6.7%, volumetric 11.5%7 |
| T/R ratio (tangential ÷ radial) | 1.91, calculated8 |
| Movement coefficients | CR 0.00119; CT 0.002345 |
How hard is aspen (quaking aspen)?
Ticks are the anchor woods, from eastern white pine to ipe; the scale is in lbf. See quaking aspen on the Janka chart.
How much does it move?
A 10-inch flat-sawn quaking aspen board going from 6% to 10% moisture content, the range the Handbook recommends for individual pieces of interior woodwork in most of the United States10, widens by 0.094 in9. A quartersawn board widens by 0.048 in9.
The coefficients apply from 6% to 14% moisture content11.
Try your own board in the wood movement calculator.
What it's used for
Aspen heartwood is grayish white to light grayish brown, and the lighter sapwood is not clearly marked off. The wood is usually straight grained, with a fine, uniform texture, and it is easily worked. It is cut for lumber, pallets, boxes and crating, pulpwood, particleboard, strand panels, excelsior, matches, veneer, and turned articles, and it is one of the preferred species for oriented strandboard.12
Compare with
Questions
- Is aspen a hardwood?
- Yes. Aspen is a hardwood13. In the Handbook, hardwood means a broad-leaved angiosperm, not a wood that is necessarily hard. Specific gravity on a 12% MC volume basis is 0.381.
- Is aspen harder than eastern white pine?
- Aspen is softer than eastern white pine: 350 lbf1 versus 380 lbf3, both at 12% moisture.
- How much does aspen shrink?
- From green to oven-dry, tangential shrinkage is 6.7% and radial shrinkage is 3.5%7. The T/R ratio is 1.91, calculated8.
References
- 1. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-9
- 2. Calculated from the 12% moisture Janka side-hardness values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 3. USDA Wood Handbook (FPL-GTR-282), Table 5-3b, p. 5-12
- 4. Calculated from the 12% moisture modulus of elasticity values in the USDA Wood Handbook (FPL-GTR-282), Tables 5-3 and 5-5.
- 5. USDA Wood Handbook (FPL-GTR-282), Table 13-5, p. 13-17
- 6. USDA Wood Handbook (FPL-GTR-282), Table 5-3a, p. 5-4
- 7. USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8
- 8. Calculated from tangential shrinkage divided by radial shrinkage (USDA Wood Handbook (FPL-GTR-282), Table 4-3, p. 4-8).
- 9. Calculated with Wood Handbook Eq. 13-3 (p. 13-16): 10 in × the coefficient × 4 percentage points. Tangential coefficient 0.00234; radial coefficient 0.00119.
- 10. USDA Wood Handbook (FPL-GTR-282), Table 13-2, p. 13-5
- 11. USDA Wood Handbook (FPL-GTR-282), ch. 13, p. 13-16
- 12. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-4
- 13. USDA Wood Handbook (FPL-GTR-282), ch. 2, p. 2-2